Factory directly supply Resistance Of The Material Of The Wire - SGHYZ high temperature electrothermal alloy – Shougang
Factory directly supply Resistance Of The Material Of The Wire - SGHYZ high temperature electrothermal alloy – Shougang Detail:
BEIJING SHOUGANG GITANE NEW MATERIALS CO.LTD has long been committed to the research and development of electric heating alloy products with good oxidation resistance and high temperature resistance. SGHYZ product is a new product developed after HRE which has been widely used in high temperature electrothermal alloy materials in recent years. Compared with HRE, SGHYZ product has higher purity and better oxidation resistance. With the special rare earth element collocation and unique metallurgical manufacturing process, the material has been recognized by domestic and foreign customers in the field of high-temperature heat-resistant fiber. It has been successfully applied in ceramic sintering, diffusion furnace, high power density and high temperature industrial kiln.
1. grades and chemical composition%
C | Si | Cr | Al | Fe |
≤0.04 | ≤0.4 | 20-23 | 5.8 | - |
2. Specifications
(1) Diameter of round wire:φ0.15-9.0mm
(2) Flat wire thickness:0.1-0.4mm Width:0.5-4.5mm
(3)Strip thickness: 0.5-2.5 Width:5-48mm
3. Delivery status
(1) The diameter of the wire is larger than 5.0 mm,Blue disc delivery
(2) Wire diameter range: 1.0-5.0 mm, golden plate delivery
(3) Wire diameter range is less than or equal to φ 1.0 mm, bright axial delivery
(4) Flat belt: delivered in polished condition.
4. Performance and Application
(1). Basic application
Maximum usetemperature℃ | Annealed tensile strength N/mm2 | Elongation % | 20℃resistancerateμ.Ω.m |
1425 |
650-800 |
>14 |
1.45 |
Application: High temperature ceramic firing furnace / high temperature heat treatment furnace / high temperature diffusion in electronic industry
(2).Characteristics
densityg/cm3 | 1000℃high temperaturestrength MPa | 1350 ℃ fast life (hoursAccording to GB / t13300-91 standard | Completely oxidized stateRadiation coefficient of |
7.1 | 20 | >80 | 0.7 |
(3)、Average linear expansion coefficient
temperature℃ | Average linear expansion coefficien×10-6/k |
20-250 |
11 |
20-500 |
12 |
20-750 |
14 |
20-1000 |
15 |
(4).Resistance temperature correction factor
temperature℃ | 700 | 900 | 1100 | 1200 | 1300 |
Ct | 1.02 | 1.03 | 1.04 | 1.04 | 1.04 |
5. Relative life
Wire specifications(mm) | Resistance(Ω/m) | Weight(g/m) |
1 | 1.85 | 5.58 |
1.1 | 1.53 | 6.75 |
1.2 | 1.28 | 8.03 |
1.3 | 1.09 | 9.42 |
1.4 | 0.942 | 10.9 |
1.5 | 0.821 | 12.5 |
1.6 | 0.721 | 14.3 |
1.7 | 0.639 | 16.1 |
1.8 | 0.57 | 18.1 |
1.9 | 0.511 | 20.1 |
2 | 0.462 | 22.3 |
2.1 | 0.419 | 24.6 |
2.2 | 0.381 | 27 |
2.3 | 0.349 | 29.5 |
2.4 | 0.321 | 32.1 |
2.5 | 0.295 | 34.9 |
2.6 | 0.273 | 37.7 |
2.7 | 0.253 | 40.7 |
2.8 | 0.235 | 43.7 |
2.9 | 0.22 | 46.9 |
3 | 0.205 | 50.2 |
3.1 | 0.192 | 53.6 |
3.2 | 0.18 | 57.1 |
3.3 | 0.17 | 60.7 |
3.4 | 0.16 | 64.5 |
3.5 | 0.151 | 68.3 |
3.6 | 0.142 | 72.3 |
3.7 | 0.135 | 76.3 |
3.8 | 0.128 | 80.5 |
3.9 | 0.121 | 84.8 |
4 | 0.115 | 89.2 |
4.1 | 0.11 | 93.7 |
4.2 | 0.105 | 98.4 |
4.3 | 0.1 | 103.1 |
4.4 | 0.095 | 108 |
4.5 | 0.0912 | 113 |
4.6 | 0.0873 | 118 |
4.7 | 0.0836 | 123 |
4.8 | 0.0801 | 128 |
4.9 | 0.0769 | 134 |
Wire specifications(mm) | Resistance(Ω/m) | Weight(g/m) |
5 | 0.0739 | 139 |
5.1 | 0.071 | 145 |
5.2 | 0.0683 | 151 |
5.3 | 0.0657 | 157 |
5.4 | 0.0633 | 163 |
5.5 | 0.061 | 169 |
5.6 | 0.0589 | 175 |
5.7 | 0.0568 | 181 |
5.8 | 0.0549 | 188 |
5.9 | 0.053 | 194 |
6 | 0.0513 | 201 |
6.1 | 0.0496 | 207 |
6.2 | 0.048 | 214 |
6.3 | 0.0465 | 221 |
6.4 | 0.0451 | 228 |
6.5 | 0.0437 | 236 |
6.6 | 0.0424 | 243 |
6.7 | 0.0411 | 250 |
6.8 | 0.0399 | 258 |
6.9 | 0.0388 | 265 |
7 | 0.0377 | 273 |
7.1 | 0.0366 | 281 |
7.2 | 0.0356 | 289 |
7.3 | 0.0346 | 297 |
7.4 | 0.0337 | 305 |
7.5 | 0.0328 | 314 |
7.6 | 0.032 | 322 |
7.7 | 0.0311 | 331 |
7.8 | 0.0303 | 339 |
7.9 | 0.0296 | 348 |
8 | 0.0288 | 357 |
8.1 | 0.0281 | 366 |
8.2 | 0.0275 | 375 |
8.3 | 0.0268 | 384 |
8.4 | 0.0262 | 393 |
8.5 | 0.0256 | 403 |
8.6 | 0.025 | 412 |
8.7 | 0.0244 | 422 |
8.8 | 0.0238 | 432 |
8.9 | 0.0233 | 442 |
SGHYZ meter resistance / weight reference table. (the above calculation data are only for reference, the resistance fluctuation range is ± 5%, and the weight varies with the size accuracy range.)
Product detail pictures:
Related Product Guide:
As a way to ideal meet up with client's desires, all of our operations are strictly performed in line with our motto "High Top quality, Competitive Cost, Fast Service" for Factory directly supply Resistance Of The Material Of The Wire - SGHYZ high temperature electrothermal alloy – Shougang , The product will supply to all over the world, such as: Sevilla, Romania, Japan, Our products are widely recognized and trusted by users and can meet continuously developing economic and social needs. We welcome new and old customers from all walks of life to contact us for future business relationships and achieving mutual success!
By Elva from Bolivia - 2018.12.11 11:26
Adhering to the business principle of mutual benefits, we have a happy and successful transaction, we think we will be the best business partner.
By Ivy from Guinea - 2018.09.23 18:44